Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 0.100 µm/m-°C @Temperature 20.0 °C |
0.0556 µin/in-°F @Temperature 68.0 °F |
Longitudinal |
Goodfellow Carbon/Epoxy Composite Tube Carbon Fiber - Epoxy Resin MatrixInformation provided by Goodfellow. |