Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | -0.600 µm/m-°C @Temperature 20.0 °C |
-0.333 µin/in-°F @Temperature 68.0 °F |
|
Cytec Thornel® T-300 12K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
CTE, linear | -0.600 µm/m-°C @Temperature 20.0 °C |
-0.333 µin/in-°F @Temperature 68.0 °F |
|
Cytec Thornel® T-300 1K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
CTE, linear | -0.600 µm/m-°C @Temperature 20.0 °C |
-0.333 µin/in-°F @Temperature 68.0 °F |
|
Cytec Thornel® T-300 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |
|||
CTE, linear | -0.600 µm/m-°C @Temperature 20.0 °C |
-0.333 µin/in-°F @Temperature 68.0 °F |
|
Cytec Thornel® T-300 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t.. |