Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 27.9 mm/min | 1.10 in/min | ASTM D635 |
DuPont™ Surlyn® 9970 Ionomer Resin, Zinc
(discontinued **) Surlyn® 9970 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Flame Spread | 28.0 mm/min @Thickness 3.17 mm |
1.10 in/min @Thickness 0.125 in |
FH3 |
LG Chemical 15NFE GPPS High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superio.. |
|||
Flame Spread | 28.0 mm/min @Thickness 3.17 mm |
1.10 in/min @Thickness 0.125 in |
FH3 |
LG Chemical MI-730 MIPS |
|||
Flame Spread | 28.0 mm/min @Thickness 3.17 mm |
1.10 in/min @Thickness 0.125 in |
FH3 |
LG Chemical MI-750 MIPS Medium impact |
|||
Flame Spread | 28.0 mm/min @Thickness 3.17 mm |
1.10 in/min @Thickness 0.125 in |
FH3 |
LG Chemical MI-770 MIPS |
|||
Flame Spread | 27.9 mm/min | 1.10 in/min | FM VSS-302 |
Multibase Multi-Flex® D 3204 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |
|||
Flame Spread | 28.0 mm/min @Thickness 3.17 mm |
1.10 in/min @Thickness 0.125 in |
FH3 |
LG Chemical 60HR HIPS Heat resistance, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include TV sets, tape recorders, vacu.. |
|||
Flame Spread | 27.9 mm/min | 1.10 in/min | ASTM D635 |
DuPont™ Surlyn® 9950 Ionomer Resin, Zinc Surlyn® 9950 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Flame Spread | 28.0 mm/min @Thickness 3.17 mm |
1.10 in/min @Thickness 0.125 in |
FH3 |
LG Chemical 15NFI GPPS High flow, Superior transparency and processability, good appearance, non-toxicity (Conforming to FDA CFR 177.1640), Excellent electrical properties, Heat resistance and chemical resistance, Superio.. |