Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 0.0100 - 24.0 mm/min | 0.000394 - 0.945 in/min | Average value: 6.26 mm/min Grade Count:4 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Flame Spread | 0.0100 mm/min | 0.000394 in/min | ISO 3795 |
Karina 804-02/39-Y-RTC Blue PVC Compound Flame retardant PVC compound recommended for electrical conduit extrusion.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Flame Spread | 0.0100 mm/min | 0.000394 in/min | ISO 3795 |
Karina 834-48/1-A-ERM-LMP Black PVC Compound Heavy metal free PVC compound recommended for extrusion of automotive profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |