Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 27.0 - 100 mm/min | 1.06 - 3.94 in/min | Average value: 51.3 mm/min Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Flame Spread | 24.0 - 100 mm/min | 0.945 - 3.94 in/min | Average value: 74.7 mm/min Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |