Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 53 mm/min @Thickness 1.00 mm |
2.1 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Delrin® 570 NC000 Acetal (POM)
(Unverified Data**) 20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler for injection molding. Delrin 570 has very high stiff.. |