Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 32 mm/min @Thickness 2.00 mm |
1.3 in/min @Thickness 0.0787 in |
US-FMVSS; ISO 3795 |
Ineos ABS Lustran® Ultra 4115 ABS Pellets (a-methylstyrene-SAN / PC-modified), Very High Heat Grade Lustran® Ultra 4115 is very high heat grade with high impact resistance and is PC-modified. It is used for the production of molded plastic articles. |
|||
Flame Spread | 32 mm/min @Thickness 1.00 mm |
1.3 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Crastin® HR5315HF BK503 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Flame Spread | 32 mm/min @Thickness 1.00 mm |
1.3 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Crastin® LW9320 BK851 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 BK851 is a 20% glass fiber reinforced black polybutylene terephthalate blend for injection mold.. |
|||
Flame Spread | 32 mm/min @Thickness 1.00 mm |
1.3 in/min @Thickness 0.0394 in |
ISO 3795 (FMVSS 302) |
DuPont Performance Polymers Crastin® LW9330 BK851 PBT+SAN