Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 20.3 mm/min | 0.799 in/min | FM VSS-302 |
Multibase Multi-Flex® A 9402 MR TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Flame Spread | 20.3 mm/min | 0.799 in/min | ASTM D635 |
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Flame Spread | 20.3 mm/min | 0.799 in/min | ASTM D635 |
DuPont™ Surlyn® PC100 Ionomer Resin, Highest Clarity, Sodium Surlyn® PC100 luxury molding resin is a "select" grade of Surlyn® 8920, controlled to achieve the highest possible optical clarity in molded perfume jars and caps. It complies with the provisions .. |
|||
Flame Spread | 20.3 mm/min | 0.799 in/min | ASTM D635 |
DuPont™ Surlyn® 9730 Ionomer Resin, Zinc
(discontinued **) Surlyn® 9730 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |