Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flame Spread | 0.000 - 38.0 mm/min | 0.000 - 1.50 in/min | Average value: 25.3 mm/min Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Flame Spread | 0.000 - 42.0 mm/min | 0.000 - 1.65 in/min | Average value: 16.4 mm/min Grade Count:8 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Flame Spread | 0.000 - 5.00 mm/min @Thickness 2.00 mm |
0.000 - 0.197 in/min @Thickness 0.0787 in |
FMVSS 302 |
SABIC Innovative Plastics ULTEM AUT200 PEI (Europe-Africa-Middle East) Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperatu.. |