Thermal Properties | Metric | English | Comments |
---|---|---|---|
Rotating Bomb Oxidation Test (RBOT) | >= 1700 min | >= 1700 min | ASTM D 2272 |
ConocoPhillips Hydroclear Diamond Class® 32 AW Turbine Oil Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser.. |
|||
Rotating Bomb Oxidation Test (RBOT) | >= 1700 min | >= 1700 min | ASTM D 2272 |
ConocoPhillips Hydroclear Diamond Class® 32 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |
|||
Rotating Bomb Oxidation Test (RBOT) | >= 1700 min | >= 1700 min | ASTM D 2272 |
ConocoPhillips Hydroclear Diamond Class® 46 AW Turbine Oil Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser.. |
|||
Rotating Bomb Oxidation Test (RBOT) | >= 1700 min | >= 1700 min | ASTM D2272 |
ConocoPhillips Hydroclear Diamond Class® 46 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |
|||
Rotating Bomb Oxidation Test (RBOT) | >= 1700 min | >= 1700 min | ASTM D 2272 |
ConocoPhillips Hydroclear Diamond Class® 68 AW Turbine Oil Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser.. |
|||
Rotating Bomb Oxidation Test (RBOT) | >= 1700 min | >= 1700 min | ASTM D2272 |
ConocoPhillips Hydroclear Diamond Class® 68 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |