Thermal Properties | Metric | English | Comments |
---|---|---|---|
Smoke Density | <= 20 min | <= 20 min | D<sub>X</sub> at 1.5 minutes; ASTM E662 |
Rogers Corporation Bisco™ BF-1000 Cellular Silicone Foam Soft, low compression set silicone foam often specified to meet safely-conscious requirements. UL recognized for flame retardance.Applications: Low closure-force gaskets and seals, Vibration and sh.. |
|||
Smoke Density | <= 20 min | <= 20 min | D<sub>X</sub> at 1.5 minutes; ASTM E662 |
Rogers Corporation Bisco™ HT-800 Cellular Silicone Foam Medium grade silicon sponge. UL recognized for flame retardance and gasketing.Applications: HID (High Intensity Discharge) lighting fixture gaskets, Battery cushion in hand-held electronic products.. |
|||
Smoke Density | <= 20 min | <= 20 min | D<sub>X</sub> at 1.5 minutes; ASTM E662 |
Rogers Corporation Bisco™ HT-820 Cellular Silicone Foam Firm grade silicone sponge. UL recognized for flame retardance.Applications: Gaskets where higher closure force is available or necessary, Cushions in heavier-load applicationsGasketing and sealing.. |
|||
Smoke Density | <= 20 min | <= 20 min | D<sub>X</sub> at 1.5 minutes; ASTM E662 |
Rogers Corporation Bisco™ HT-840 Cellular Silicone Foam Extra firm grade silicone sponge. UL recognized of flame retardance.Applications: High closure-force gaskets, Press-pads where conformable imprinting support is required, such as decal lamination o.. |
|||
Smoke Density | <= 20 min | <= 20 min | D<sub>X</sub> at 1.5 minutes; ASTM E662 |
Rogers Corporation Bisco™ HT-870 Cellular Silicone Foam Gasketing and sealing rating is JMLU-2 (Listed) per UL 157. No UV degradation per SAE J-1960. Ozone effect rating is 0 (no cracks) per ASTM D-1171. No staining per ASTM D-925(A). Passes AMS-3568.. |
|||
Smoke Density | 20 min | 20 min | ASTM E-84-95 |
Dow Saran® 540 Vapor Retarder Film Saran™ Vapor Retarder Film is a biaxially oriented barrier film designed as a water vapor retarder for insulation applications. It is available in 400 gauge. Roll size: 35.5" x 375 long.Informat.. |