Thermal Properties Metric English Comments
Decomposition Temperature 382 - 393 °C
720 - 739 °F
1% Wt. Loss in Air; TGA
Solvay Specialty Polymers Hylar® 5000 HG Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Hylar® 5000 HG is a crystalline high molecular weight powder form of polyvinylidene fluoride specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong..
Decomposition Temperature 382 - 393 °C
720 - 739 °F
1% Wt. loss. Air; TGA
Shanghai Ofluorine T-1 PVDF for coatings (DF-1)
Description: T-1 PVDF for coatings is solid powder, it can mixed with acrylic resin, additive, and become superior performance baking PVDF fluorocarbon coatings. Compared with other grade of PVDF, T..
Decomposition Temperature 382 - 393 °C
720 - 739 °F
1% Wt. Loss in Air; TGA
Solvay Specialty Polymers Hylar® 5000 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Hylar 5000 is a crystalline high molecular weight powder form of polyvinylidene fluoride specifically designed for solvent-based coatings to provide improved gloss. It forms mechanically strong and ..