Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 345 °C | 653 °F | Degradation Temperature; TGA |
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy Product Description: EPO-TEK® 377H is a two component, high Tg, graphite filled epoxy designed for ESD/EMI shielding of semiconductor devices and electronics. It can be used in many electronic ind.. |
|||
Decomposition Temperature | 345 °C | 653 °F | 5% weight loss; TGA; IPC-TM-650.2.4.24.6 |
Park Electrochemical Nelco® N4000-11 BC® Buried Capacitance™ Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |
|||
Decomposition Temperature | 345 °C | 653 °F | 5% weight loss; TGA; IPC-TM-650.2.4.24.6 |
Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |