Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 325 °C | 617 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® 301-2FL Low Stress, Optical Epoxy Product Description: EPO-TEK® 301-2FL is a two component optical, medical, and semiconductor grade epoxy resin. It is a more flexible version of EPO-TEK® 301-2.Advantages & Application Notes: Sug.. |
|||
Decomposition Temperature | 325 °C | 617 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® EV2118-2 Silver-filled, electrically conductive epoxy Preliminary Product Information SheetMaterial Description: A silver-filled, electrically conductive epoxy designed for semiconductor and electronic assembly.Information Provided by Epoxy Technology |
|||
Decomposition Temperature | 325 °C | 617 °F | 5% weight loss; TGA; IPC-TM-650.2.4.24.6 |
Park Electrochemical Nelco® N4000-6 FC Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-6 FC is a high-Tg epoxy laminate and prepreg system that provides a wide range of performance versatility and ease of processing for demanding high-layer count applications.Key Fea.. |