Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 318 °C | 604 °F | |
DayGlo Gem-Tone GC-13P Ruby Red Gem-Tone® GC-13P Ruby Red is a rich, strong blue shade red colorant intended for use in clarified polypropylene. Clean, haze free, non-warping color formulations can easily be achieved with the use.. |