Thermal Properties Metric English Comments
Decomposition Temperature >= 85.0 °C
>= 185 °F
Avoid temperature > 80°C except during use
Synergy Polymers Ultra Purge HIGH-E
Best with color changes and material changes. Cleans out barrels, nozzles, hot runners, and heads of extruders from carbon remnants, deposits and incrustations. Has expanding agents to help in clean..
Decomposition Temperature >= 85.0 °C
>= 185 °F
Avoid temperature > 80°C except during use
Synergy Polymers Ultra Purge HT
Best with color changes and material changes. Cleans out barrels, nozzles, hot runners, and heads of extruders from carbon remnants, deposits and incrustations. Has expanding agents to help in clean..
Decomposition Temperature >= 85.0 °C
>= 185 °F
Avoid temperature > 80°C except during use
Synergy Polymers Ultra Purge LOW-E
Best with color changes and material changes. Cleans out barrels, nozzles, hot runners, and heads of extruders from carbon remnants, deposits and incrustations. Has expanding agents to help in clean..
Decomposition Temperature >= 85.0 °C
>= 185 °F
Avoid temperature > 80°C except during use
Synergy Polymers Ultra Purge Plus
Best with color changes and material changes. Cleans out barrels, nozzles, hot runners, and heads of extruders from carbon remnants, deposits and incrustations. Has expanding agents. Moldable compou..
Decomposition Temperature >= 85.0 °C
>= 185 °F
Avoid temperature > 80°C except during use
Synergy Polymers Ultra Purge P-O
Ultra Purge is a specially designed cleaning compound that comes premixed and ready-to-use in pellet form. It cleans black specks and deposits from screws, barrels, nozzle, hot runners and heads of ..