Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 375 - 400 °C | 707 - 752 °F | Thermal Stability via TGA : beginning - and at 1% weight loss in air |
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound
(discontinued **) Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Decomposition Temperature | 330 - 400 °C | 626 - 752 °F | Thermal Stability via TGA : beginning - and at 1% weight loss in air |
Solvay Specialty Polymers Solef® 8808/0902 Carbon Fiber Reinforced PVDF Compound
(discontinued **) Key features of this grade: Carbon Fiber Reinforcement, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinate.. |
|||
Decomposition Temperature | 375 - 400 °C | 707 - 752 °F | ASTM E1131 |
Zeus PVDF Tubing PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char.. |
|||
Decomposition Temperature | 375 - 400 °C | 707 - 752 °F | Thermal Stability via TGA : beginning - and at 1% weight loss in air |
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Decomposition Temperature | 375 - 400 °C | 707 - 752 °F | Thermal Stability via TGA : beginning - and at 1% weight loss in air |
Solvay Specialty Polymers Solef® 1009 PVDF Homopolymer
(discontinued **) Key features of this grade: Mean Viscosity, All Purpose, Injection/Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SO.. |
|||
Decomposition Temperature | 375 - 400 °C | 707 - 752 °F | Thermal Stability via TGA : beginning - and at 1% weight loss in air |
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Decomposition Temperature | 375 - 400 °C | 707 - 752 °F | Thermal Stability via TGA : beginning - and at 1% weight loss in air |
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |