Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | 261 °C | 502 °F | Degradation Temperature |
Epoxy Technology EPO-TEK® 302 Fast Setting, Optical Epoxy Product Description: EPO-TEK® 302 is a two component, fast-gelling, room temperature curing epoxy, designed for electronic, optical, medical, and general applications. Advantages & Application No.. |