Thermal Properties | Metric | English | Comments |
---|---|---|---|
Decomposition Temperature | >= 100 °C | >= 212 °F | |
BASF Palusol® 100 Silicate Panel Relevant identified uses: Intumescent plates for use as fire protection in the building industryInformation provided by BASF |
|||
Decomposition Temperature | >= 100 °C | >= 212 °F | |
BASF Palusol® 104 Silicate Panel Relevant identified uses: Intumescent plates for use as fire protection in the building industryInformation provided by BASF |
|||
Decomposition Temperature | >= 100 °C | >= 212 °F | |
BASF Palusol® SW 60-1 FSC 100% Silicate Panel Information provided by BASF |
|||
Decomposition Temperature | >= 100 °C | >= 212 °F | |
BASF Palusol® 210 Silicate Panel Relevant identified uses: Intumescent plates for use as fire protection in the building industryInformation provided by BASF |