Polymer Property : Flash Point = 82.4 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 28.0 °C
82.4 °F
Seta
Lord Adhesives Flocklok® Catalyst 1
Flocklok Catalyst 1 will accelerate the cure rate of Flocklok adhesives and will not diminish the work life, unless exposed to moisture. There is minimal impact on VOC levels, as low levels of the c..
Flash Point 28.0 °C
82.4 °F
Solvay GERONOL® FF/4 Surfactant
Description: Multipurpose emulsifier for agrochemical formulations. Used in pair with Geronol FF/6-C or MS-C.Identification: BLENDED EMULSIFIERSSolubility: Dispersible in water. Soluble in most pola..
Flash Point 28.0 °C
82.4 °F
Solvay GEROPON® DOS Surfactant
Description: Anionic wetting agent. Compliant with the EU's detergent biodegradability regulation.Identification: SODIUM DIOCTYLSULPHOSUCCINATE IN HYDROALCOHOLIC SOLUTIONSolubility: Dispersible in w..
Flash Point 28.0 °C
82.4 °F
Solvay RHODACAL® 70/B Surfactant
Description Anionic, linear Calcium dodecylbenzene sulfonate, 70% active , useful in emulsifier blendsIdentification: MIXTURE OF LINEAR DODECYLBENZENSULPHONIC ACID, CALCIUM SALT AND ISOBUTYL ALCOHOL..
Flash Point 28.0 °C
82.4 °F
Solvay RHODACAL® 60/B Surfactant
Description: Linear Calcium dodecylbenzene sulfonate, 60% active , useful in emulsifier blends where low viscosity is needed.Identification: MIXTURE OF LINEAR DODECYLBENZENSULPHONIC ACID, CALCIUM S..
Flash Point >= 28.0 °C
>= 82.4 °F
closed cup
Dow Corning SYL-OFF® 292 COATING
Syl-Off® 292 Coating is one of several alternative base polymers for use in Syl-Off solvent-based, tin-catalyzed release coatings. It is a 30 percent solids dispersion of a blend of reactive siloxa..
Flash Point 28.0 °C
82.4 °F
closed cup
3M AC-132 Adhesion Promoter
3M Adhesion Promoter AC-132 is a surface treatment to speed and promote adhesion of polysulfide and polythioether sealants to metals and/or solvent-resistant coatings. It contains mixed solvents ble..