Flash Point 16.1 °C
61.0 °F
Setaflash, Closed Cup; ASTM D3278-82
Lord Adhesives Aeroglaze® Z302 Absorptive Polyurethane
Aeroglaze® Z302 absorptive polyurethane is primarily for application to substrates used in space operations. These operations include those where coatings must exhibit low outgassing characterist..