Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 316 °C | 600 °F | |
ConocoPhillips Inca® 1000 Oil, AGMA No. 8A Comp. Description: Conoco Inca Oil is a high-quality compounded lubricant recommended for use in heavily loaded industrial and automotive worm gears and bearings operating at moderate to high temperatures.. |
|||
Flash Point | >= 316 °C | >= 600 °F | ASTM D 92 |
ConocoPhillips 680 Bearing Oil Description: Conoco Bearing Oil is formulated for the circulating systems that lubricate roll-neck bearings in steel and nonferrous rolling mills. It is suited for systems in which water and corrosi.. |