Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 266 °C | 511 °F | ASTM D92 |
ExxonMobil 312 Mobilgard 12 Series Mobilgard 12 Series by ExxonMobil are high performance diesel engine oils developed for use in trunk piston engines operating on low sulphur distillate fuels in marine and industrial applications. T.. |
|||
Flash Point | 266 °C | 511 °F | ASTM D92 |
ExxonMobil 68 Mobil EAL Envirosyn H Series Mobil EAL Envirosyn H Series oils are super premium, high performance fully synthetic environmentally aware hydraulic and circulating oils designed to provide outstanding performance in systems oper.. |
|||
Flash Point | 266 °C | 511 °F | |
ChevronTexaco Canopus® 150 Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant .. |
|||
Flash Point | 266 °C | 511 °F | ASTM D92 |
ChevronTexaco ParaMount™ 6005 Paraffinic Process Oil FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur.. |
|||
Flash Point | 266 °C | 511 °F | ASTM D92 |
ExxonMobil 312 Mobilgard 12 Series Mobilgard 12 Series by ExxonMobil are high performance diesel engine oils developed for use in trunk piston engines operating on low sulphur distillate fuels in marine and industrial applications. T.. |
|||
Flash Point | 266 °C | 511 °F | ASTM D92 |
ExxonMobil SAE 30 Mobilgard 300 Mobilgard 300 by ExxonMobil is a premium quality, extra high performance system oil designed for crosshead diesel engines. High quality paraffinic base oils along with a balanced additive system pro.. |
|||
Flash Point | 266 °C | 511 °F | |
Duratherm G Polyalkylenev Glycol Heat Transfer Fluid Glycol fluids such as Ucon 500(TM) have been used for years but have, until now offered very little protection from negative elements such as oxidation. Duratherm G also has reduced odors and improv.. |
|||
Flash Point | 266 °C | 511 °F | COC; ASTM D92 |
ExxonMobil SpectraSyn™ 10 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |
|||
Flash Point | 266 °C | 511 °F | ASTM D92 |
ExxonMobil 68 Mobil EAL Envirosyn H Series Mobil EAL Envirosyn H Series oils are super premium, high performance fully synthetic environmentally aware hydraulic and circulating oils designed to provide outstanding performance in systems oper.. |
|||
Flash Point | 266 °C | 511 °F | ASTM D92 |
ExxonMobil SAE 30 Mobilgard 300 Mobilgard 300 by ExxonMobil is a premium quality, extra high performance system oil designed for crosshead diesel engines. High quality paraffinic base oils along with a balanced additive system pro.. |