Polymer Property : Flash Point = 51.8 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Flash Point 11.0 °C
51.8 °F
Seta
Lord Adhesives Chemlok® Y-1520A Adhesive
LORD Chemlok® Y-1520A adhesive is a clear, one-coat adhesive used to bond specialty elastomers to metal and plastics during vulcanization of the rubber. Chemlok Y-1520A adhesive is useful for bon..
Flash Point 11.0 °C
51.8 °F
closed cup
Lucite International Colacryl ® TS1173 Reactive Acrylic Syrup
Lucite® Colacryl® TS1173 is a reactive polymer solution containing dissolved polymers, plasticiser and a polymerisation activator.Information provided by Lucite International
Flash Point 11.0 °C
51.8 °F
Seta
LyondellBasell TEBOL® 99 High Purity TBA, Tertiary butyl alcohol
Information provided by Lyondell.
Flash Point 11.0 °C
51.8 °F
Indium Corp. Indalloy® 84004 Flux #4-0A Clear Liquid Flux
Indalloy Flux #4-0A is a clear liquid flux formulated for the purpose of soldering moderately easy to difficult metallizations such as nickel, oxidized copper, Kovar and brass. This flux contains o..
Flash Point 11.0 °C
51.8 °F
closed cup
Dow Corning 1-6136 ANTISTAT
Dow Corning 1-6136 Antistat is a cationic alkoxy silane and is designated 3-trimethoxysilylpropyloctadecyidimethyl ammonium chloride. It is supplied as a 42 percent active solution (by weight) in me..
Flash Point 11.0 °C
51.8 °F
BASF 1,4-Dioxane
Formula: C
Flash Point 11.0 °C
51.8 °F
BASF 1,4-Dioxane stab
Formula: C4H8O2CAS: 123.91.1Description: 1,4-Dioxane stab. is a colorless to yellow liquid, with an ether-like odor. It is miscible with water and other organic solvents. Synonyms: p-Dioxan, Dioxan..