Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 10.0 °C | >= 50.0 °F | ASTM D56 |
Humiseal 1C63 Silicone Conformal Coating Humiseal 1C63 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses thermal shock .. |
|||
Flash Point | 10.0 °C | 50.0 °F | closed cup |
Dow Corning 1890 PROTECTIVE COATING Silicone RTV in solvent dispersionInformation provided by Dow Corning |
|||
Flash Point | 10.0 °C | 50.0 °F | closed cup |
Dow Corning Z-6689 WATER REPELLENT Dow Corning® Z-6689 Water Repellent is a solvent-free silane/ siloxane concentrate, dilutable in organic or silicone solvents to formulate a water repellent. Upon proper application, the formulated.. |
|||
Flash Point | >= 10.0 °C | >= 50.0 °F | closed cup |
Dow Corning 236 DISPERSION Flowable (as supplied) silicone RTV coatingInformation provided by Dow Corning |
|||
Flash Point | 10.0 °C | 50.0 °F | |
BASF Ethyl Chloroformate Formula: C3H5ClO2CAS: 541-41-3Description: Ethyl Chloroformate is a colorless to yellowish liquid with a pungent odor. It hydrolyses in the presence of water.Synonyms: Chloroformic acid ethyl ester.. |
|||
Flash Point | >= 10.0 °C | >= 50.0 °F | A Component; ASTM D92 |
Aptek 2214-A/B Low modulus urethane ESD coating/adhesive Space Grade, Low modulus urethane ESD coating/adhesiveAPTEK is a carbon-filled, thixotropic, two component, electrically conductive, flexible urethane coating/adhesive designed to dissipate an elect.. |
|||
Flash Point | 10.0 °C | 50.0 °F | A Component; ASTM D92 |
Aptek 2503R-A/B Premeasured conformal urethane coating repair kit APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electrical/electronic components.. |
|||
Flash Point | 10.0 °C | 50.0 °F | A Component; ASTM D92 |
Aptek 2506-A/B Room temperature curing, low modulus urethane conformal coating Room temperature curing, low modulus urethane conformal coatingAPTEK 2506-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the e.. |