Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 243 °C | 469 °F | open cup |
Dow Corning 705 DIFFUSION PUMP FLUID A colorless, penta phenyltrisiloxane, single-component fluid designed for ultrahigh vacuums of 10-10 torr (untrapped) and 10-11 (trapped).Information provided by Dow Corning |
|||
Flash Point | 243 °C | 469 °F | |
ChevronTexaco Compound H Rust Proof Texaco Rust Proof Compounds deliver value through:Excellent long-term rust protection — Petrolatum and special additive system form a nonhardening, self sealing film to protect surfaces against the.. |
|||
Flash Point | 243 °C | 469 °F | ASTM D92 |
ChevronTexaco FM ISO 460 Lubricating Oil Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr.. |
|||
Flash Point | 243 °C | 469 °F | COC |
ConocoPhillips Hydroclear Diamond Class® 68 AW Turbine Oil Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser.. |
|||
Flash Point | 243 °C | 469 °F | |
ConocoPhillips Hydroclear® 30 Power-D E.O. 30 Description: Conoco Hydroclear Power-D Engine Oil, formulated from Conoco's premium hydrocracked base stock, protects diesel and gasoline engines against wear, deposits, varnish, rust and corros.. |
|||
Flash Point | 243 °C | 469 °F | |
ConocoPhillips Hydroclear® 50 Power-D E.O. 50 Description: Conoco Hydroclear Power-D Engine Oil, formulated from Conoco's premium hydrocracked base stock, protects diesel and gasoline engines against wear, deposits, varnish, rust and corros.. |
|||
Flash Point | 243 °C | 469 °F | Open cup |
Dow Corning PH-1555 HRI Cosmetic Fluid A trimethyl pentaphenyl trisiloxane which provides ultra high refractive index for use in skincare, suncare, hair care, color cosmetic, and antiperspirant / deodorant applications.INCI Name: Trimeth.. |
|||
Flash Point | 243 °C | 469 °F | |
ChevronTexaco Crater® 2X Texaco Crater lubricants delivers value through:Low environmental impact — Contains a carrier solvent that is a non-ozone depleting diluent.Good water resistance — Strong resistance to water washo.. |
|||
Flash Point | 243 °C | 469 °F | COC |
ConocoPhillips Hydroclear Diamond Class® 68 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |