Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil 65 Exxon Aviation Oil EE Series Aviation Oil EE is the brand name of a premium quality line of ashless-dispersant piston engine oils. Formulated with select, highly refined base oils together with ashless-dispersant and anti-oxida.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil 15W-40 Exxon XD-3 Exxon XD-3 10W-30 and 15W-40 are premium diesel engine oils formulated to provide excellent protection to modern, high performance diesel engines used in severe on and off-highway applications. Thes.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil 22M Mobilgear SHC Mobilgear SHC 22M and 46M are supreme performance ultra high viscosity synthetic lubricants designed specifically for use in heavily loaded, low speed gears where boundary lubrication conditions oft.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil 50 Mobiltrans HD Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4. This product line .. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil Teresstic 68 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Flash Point | 240 °C | 464 °F | |
ConocoPhillips Syncon® 320 Synthetic EP Gear Oil, AGMA No. 6EP Syncon EP Plus Gear Oil is a premium quality, synthetic, extreme-pressure industrial gear lubricant developed for the lubrication of enclosed gear drives and heavily loaded plain or rolling-element .. |
|||
Flash Point | 240 °C | 464 °F | |
ConocoPhillips Syncon® 460 Synthetic EP Gear Oil, AGMA No. 7EP Syncon EP Plus Gear Oil is a premium quality, synthetic, extreme-pressure industrial gear lubricant developed for the lubrication of enclosed gear drives and heavily loaded plain or rolling-element .. |
|||
Flash Point | 240 °C | 464 °F | |
ConocoPhillips Syncon® 680 Synthetic EP Gear Oil, AGMA No. 8EP Description: Conoco Syncon Synthetic EP Gear Oil is a synthetic polyalphaolefin (PAO) lubricant for enclosed gear sets requiring extreme-pressure gear oils and operating at high temperatures. It is .. |
|||
Flash Point | 240 °C | 464 °F | |
ChevronTexaco 13 SG Diesel Engine Oil Texaco Diesel Engine Oils deliver value through:Ability to maximize oil and filter lifeImproved wear controlExtended drainsExtends oil drains in new low oil consumption GE locomotives, reducing oil .. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ChevronTexaco FM ISO 46 Synthetic Compressor Oil FeaturesChevron Synthetic Compressor Oil FM is a PAO based, synthetic, food grade, compressor oil.Although Chevron Synthetic Compressor Oil FM offers a reduced risk of fires and explosions, it is no.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ChevronTexaco Gear Compounds EP, ISO 150 FeaturesChevron Gear Compounds EP are multipurpose gear lubricants.They provide good thermal stability, extreme pressure
protection, antiwear and demulsibility, oxidation, rust, corrosion control an.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ChevronTexaco Supreme SAE 5W-30 Synthetic Motor Oil FeaturesChevron Supreme 100% Synthetic Motor Oils are designed for those drivers who demand the ultimate in engine protection. They provide an extra measure of protection for the investment in a spo.. |
|||
Flash Point | 240 °C | 464 °F | |
ChevronTexaco Syn-Star® 320 Chain Oil Texaco Syn-Star Chain Oil 320 is a chain oil designed for use in extreme high and low temperature operations. It is formulated with synthetic base oils and an additive package which provides rust an.. |
|||
Flash Point | 240 °C | 464 °F | |
ChevronTexaco Taro® 40 XL SAE 40 Texaco Taro 40 XL delivers value through:Wear protection — Performance results in the latest design medium speed trunk piston diesel engines have shown that the high level of alkalinity of this lub.. |
|||
Flash Point | 240 °C | 464 °F | |
ChevronTexaco Taro® 50 XL SAE 40 Texaco Taro 50 XL delivers value through:Wear protection — Performance results in the latest design medium speed trunk piston diesel engines have shown that the high level of alkalinity of this lub.. |
|||
Flash Point | 240 °C | 464 °F | |
ChevronTexaco Texatherm® Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging .. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil 100 Mobil DTE PM Series Mobil DTE PM Series products are high-quality, high-performance lubricants specifically designed for demanding industrial paper machine circulating systems. They are engineered to provide exceptiona.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil 10W-30 Exxon XD-3 Exxon XD-3 10W-30 and 15W-40 are premium diesel engine oils formulated to provide excellent protection to modern, high performance diesel engines used in severe on and off-highway applications. Thes.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil 150 Mobilgear SHC XMP Series Mobilgear SHC XMP Series supreme performance, fully synthetic industrial gear oils designed to provide optimum equipment protection and oil life even under extreme conditions. Mobil polyalphaolefin .. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil 20W-50 Exxon Aviation Oil Aviation Oil 100, 120 and 20W-50 are non-dispersant, mineral oil-based lubricants for piston engines of commercial, military and private aircraft. They contain very low concentrations of anti-oxid.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil 22M Mobilgear SHC Mobilgear SHC 22M and 46M are supreme performance ultra high viscosity synthetic lubricants designed specifically for use in heavily loaded, low speed gears where boundary lubrication conditions oft.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil 26M Mobilgear SHC Mobilgear SHC 22M and 46M are supreme performance ultra high viscosity synthetic lubricants designed specifically for use in heavily loaded, low speed gears where boundary lubrication conditions oft.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil Mobil Synthetic Oven Lube 1090 Mobil Synthetic Oven Lube 1090 is a supreme performance synthetic high temperature lubricant designed specifically for lubrication of hot conveyor chains in drying ovens and similar severe applicati.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D-92 |
ConocoPhillips ANDEROL® 6680 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Flash Point | 240 °C | 464 °F | ASTM D-92 |
ConocoPhillips ANDEROL® FGC 30 Synthetic Food Grade Compressor Fluid, ISO 68 Description: ANDEROL FGC Series Compressor Fluids are synthetic hydrocarbon (PAO) based lubricants formulated for use in compressors. FGC Series Fluids meet the former H-1 approval requirements of t.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D-92 |
ConocoPhillips ANDEROL® PQ AA 85W140 White Mineral Food Grade Gear Oil, ISO Grade 320, SAE Gear Oil Grade 85W140 Description: ANDEROL PQ AA Series Gear Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Gear.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil 50 Mobiltrans HD Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4. This product line .. |
|||
Flash Point | 240 °C | 464 °F | |
BASF Palatinol® N Diisononyl Phthalate Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D-92 |
ConocoPhillips ANDEROL® FGH 32 Synthetic Food Grade Hydraulic Fluid, ISO 32 Description: ANDEROL FGH Series Hydraulic Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA wh.. |