Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 235 °C | >= 455 °F | |
Parker Chomerics CHO-BOND 1011, Part B Information provided by Chomerics |
|||
Flash Point | 235 °C | 455 °F | |
Lubriplate SYNAC 68 Diester-Based Synthetic Air Compressor Fluid These diester-based synthetic air compressor fluids are outstanding for applications where the fluid is subjected to high temperature and high stress conditions over extended drain intervals.Synac S.. |
|||
Flash Point | 235 °C | 455 °F | |
Lubriplate SYNAC 46 Diester-Based Synthetic Air Compressor Fluid These diester-based synthetic air compressor fluids are outstanding for applications where the fluid is subjected to high temperature and high stress conditions over extended drain intervals.Synac S.. |
|||
Flash Point | 235 °C | 455 °F | ASTM D92 |
ExxonMobil 627 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Flash Point | 235 °C | 455 °F | ASTM D92 |
ExxonMobil 630 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Flash Point | 235 °C | 455 °F | ASTM D92 |
ExxonMobil Spartan EP 100 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |
|||
Flash Point | 235 °C | 455 °F | ASTM D92 |
ChevronTexaco 1000 THF Tractor Hydraulic Fluid FeaturesChevron 1000 THF (formerly Chevron Tractor Hydraulic Fluid and Amoco 1000 Fluid) is a high quality, multifunctional fluid, specially formulated for use in transmissions, final drives, wet br.. |
|||
Flash Point | 235 °C | 455 °F | |
ChevronTexaco 68 AW Hydraulic Oil Texaco AW Hydraulic Oils deliver value through:High oxidation stability — Longer service life than with conventional lubricants in high pressure service.Rust and corrosion protection — Gives excel.. |
|||
Flash Point | 235 °C | 455 °F | ASTM D92 |
ChevronTexaco ISO 68 Hydraulic Oil AW FeaturesChevron Hydraulic Oils AW are designed to give excellent hydraulic pump protection. They are formulated with refined paraffinic base oils. They provide excellent antiwear protection, oxidati.. |
|||
Flash Point | 235 °C | 455 °F | [°C] Fire Point |
ChevronTexaco Quenchtex® A Texaco Quenchtex oils deliver value through:Controlled cooling of metals — Combines the high initial quenching speed of water with slow final quenching speed of oil.Safety — High flash point and f.. |
|||
Flash Point | 235 °C | 455 °F | |
ChevronTexaco Rando® HD 68 Texaco Rando HD oils deliver value through:Longer equipment life — Special antiwear additive package reduces wear by protecting surfaces when load causes breakdown of the lubricant film.Reduced dow.. |
|||
Flash Point | 235 °C | 455 °F | ASTM D92 |
ChevronTexaco Rykon® ISO 68 Oil AW FeaturesChevron Rykon Oils AW are designed to give maximum hydraulic pump protection.Chevron Rykon Oils AW are formulated with ISOSYN® base stocks.They provide excellent antiwear protection, oxidat.. |
|||
Flash Point | 235 °C | 455 °F | |
ChevronTexaco TDH® Oil Texaco TDH oils deliver value through:Lower operating costs — By delivering or exceeding the performance of fluids supplied by equipment manufacturers, helps in avoiding the cost of generally more .. |
|||
Flash Point | 235 °C | 455 °F | |
ChevronTexaco TDH® Special Oil Texaco TDH Oil Special delivers value through:Lower operating costs — By delivering or exceeding the performance of fluids supplied by equipment manufacturers, helps in avoiding the cost of general.. |
|||
Flash Point | 235 °C | 455 °F | ASTM D92 |
ExxonMobil 627 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Flash Point | 235 °C | 455 °F | ASTM D92 |
ExxonMobil Spartan EP 100 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |
|||
Flash Point | 235 °C | 455 °F | |
ConocoPhillips El Mar® Grade 15W-40 Geo Oil Description: Conoco El Mar® Geo Oil is a high-quality, rust- and oxidation-inhibited, nondetergent, ashless gas engine oil. It is formulated with high viscosity index paraffinic base oils blended w.. |
|||
Flash Point | 235 °C | 455 °F | |
ConocoPhillips Hydroclear® 68 2 EP gear Oil Description: Conoco Hydroclear EP Gear Oil is a premium extreme-pressure industrial gear lubricant with superior deposit control. Hydroclear EP Gear Oil is specially formulated with proprietary addi.. |
|||
Flash Point | 235 °C | 455 °F | ASTM D92 |
ExxonMobil 630 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Flash Point | 235 °C | 455 °F | |
ConocoPhillips 68 Gear Oil AGMA Lubricant No. 2 EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Flash Point | 235 °C | 455 °F | |
ConocoPhillips Hydroclear® 100 3 EP gear Oil Description: Conoco Hydroclear EP Gear Oil is a premium extreme-pressure industrial gear lubricant with superior deposit control. Hydroclear EP Gear Oil is specially formulated with proprietary addi.. |
|||
Flash Point | 235 °C | 455 °F | COC |
ConocoPhillips Conoco® El Mar® Ashless Heavy Duty Oil, SAE Viscosity Grade 15W-40 Conoco® El Mar Ashless Heavy Duty is a high-quality, ashless, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged 2-stroke cycle natural gas engi.. |