Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 218 °C | 424 °F | ASTM D92 |
ExxonMobil 16M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Flash Point | 218 °C | 424 °F | ASTM D92 |
ExxonMobil Light Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Flash Point | >= 218 °C | >= 424 °F | ASTM D92 |
ExxonMobil Mobilarma 524 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |
|||
Flash Point | 218 °C | 424 °F | ASTM D92 |
ExxonMobil Mobil Vaculine 1409 Mobil Vacuoline 1400 Series oils are extra high performance lubricants specifically designed to satisfy the requirements of machine tools that use one oil for both hydraulic systems and way lubricat.. |
|||
Flash Point | 218 °C | 424 °F | |
ConocoPhillips Syncon® 22 Synthetic AW Hydraulic Fluid 22 Syncon AW Hydraulic Fluid is a premium quality, synthetic antiwear hydraulic fluid developed for use in industrial and mobile equipment operating at extreme temperatures. It is particularly recommen.. |
|||
Flash Point | 218 °C | 424 °F | |
ChevronTexaco Crater® 0 Texaco Crater lubricants delivers value through:Low environmental impact — Contains a carrier solvent that is a non-ozone depleting diluent.Good water resistance — Strong resistance to water washo.. |
|||
Flash Point | 218 °C | 424 °F | ASTM D92 |
ChevronTexaco ISO 100 Red Chain Bar Oil FeaturesChevron Red Chain Bar Oils are very tacky, tough, lubricants made from special high viscosity base oils having the desired flow and pumpability properties to assure adequate lubrication over.. |
|||
Flash Point | 218 °C | 424 °F | ASTM D92 |
ChevronTexaco ISO 150 Red Chain Bar Oil FeaturesChevron Red Chain Bar Oils are very tacky, tough, lubricants made from special high viscosity base oils having the desired flow and pumpability properties to assure adequate lubrication over.. |
|||
Flash Point | 218 °C | 424 °F | ASTM D92 |
ChevronTexaco ISO 220 Red Chain Bar Oil FeaturesChevron Red Chain Bar Oils are very tacky, tough, lubricants made from special high viscosity base oils having the desired flow and pumpability properties to assure adequate lubrication over.. |
|||
Flash Point | 218 °C | 424 °F | ASTM D92 |
ChevronTexaco NLGI 1 Moly MAX Grease EP FeaturesChevron Moly MAX Greases EP are high performance greases.They are formulated with extreme pressure additives and 5% molybdenum disulfide (moly). They are dark gray/black in color and smooth .. |
|||
Flash Point | 218 °C | 424 °F | See Note 3. |
ChevronTexaco PremiumRB Texaco Premium RB delivers value through:Wide application range — Suitable for high rpm operation, operating temperatures ranging from -34°C to 177°C (-30°F to 350°F) and offers excellent rust .. |
|||
Flash Point | 218 °C | 424 °F | |
ChevronTexaco Syn-Star® GL SAE 80W-140 Texaco Syn-Star GL oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oil used in these products provides outstanding stability.Extended drain cap.. |
|||
Flash Point | 218 °C | 424 °F | ASTM D92 |
ExxonMobil Light Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Flash Point | 218 °C | 424 °F | ASTM D92 |
ExxonMobil Mobil Vaculine 1409 Mobil Vacuoline 1400 Series oils are extra high performance lubricants specifically designed to satisfy the requirements of machine tools that use one oil for both hydraulic systems and way lubricat.. |
|||
Flash Point | >= 218 °C | >= 424 °F | ASTM D92 |
ExxonMobil Mobilarma 524 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |
|||
Flash Point | 218 °C | 424 °F | |
ConocoPhillips HD Fleet™ 20W20 Engine Oil Description: Conoco HD Fleet Engine Oil is a high-quality, single-grade oil formulated from Conoco's premium hydrocracked base stock and unique additive technology. This oil is highly recommende.. |
|||
Flash Point | 218 °C | 424 °F | |
ConocoPhillips Hydroclear® 5W-30 Super All Season and Super Motor Oil Description: Conoco Hydroclear Super All Season and Super Motor Oils, formulated with premium base stocks, lubricate domestic and imported passenger cars, sport-utility vehicles, light-duty trucks, .. |
|||
Flash Point | 218 °C | 424 °F | |
ChevronTexaco Cepheus® 220 Texaco Cepheus oil deliver value throughThe ability to retain lubrication properties in the presence of water.Good rust protection from a carefully designed additive package.The ease with which they.. |
|||
Flash Point | 218 °C | 424 °F | |
ChevronTexaco Chain, Bar, and Sprocket Lubricant Texaco Chain, Bar and Sprocket Lubricant delivers value through:Reduced wear — Minimize wear for the chain, bar, and sprocket.Tackiness — The increased tackiness additive keeps the oil on the chai.. |
|||
Flash Point | 218 °C | 424 °F | |
ChevronTexaco Summer Chain Bar Oil Texaco Chain Bar Oil Summer Grade delivers value through:Reduced wear — Minimize wear for the chain, bar, and sprocket.Tackiness — The increased tackiness additive keeps the oil on the chain and p.. |
|||
Flash Point | 218 °C | 424 °F | ASTM D92 |
ExxonMobil 16M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Flash Point | 218 °C | 424 °F | |
ConocoPhillips HD Fleet™ 10W Engine Oil Description: Conoco HD Fleet Engine Oil is a high-quality, single-grade oil formulated from Conoco's premium hydrocracked base stock and unique additive technology. This oil is highly recommende.. |
|||
Flash Point | 218 °C | 424 °F | ASTM D92 |
ChevronTexaco Bright-Cut® AM Metal Working Fluid FeaturesChevron Bright-Cut Metalworking Fluids are a complete line of chlorine-free cutting oils that offer benefits not found in conventional cutting oils.The unique synthetic antiweld components .. |