Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 171 °C | >= 340 °F | Closed Cup (D93) |
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-he.. |
|||
Flash Point | >= 171 °C | >= 340 °F | pmcc - Pensky-Martens Closed Cup; ASTM D93 |
Paratherm Corporation Paratherm™ HT Heat Transfer Fluid Paratherm HT Heat Transfer Fluid is a partially hydrogenated terphenyl based product designed for closed-loop liquid phase heating to 650°F (343°C) in fired heaters and 675°F (358°C) in solid fu.. |
|||
Flash Point | 171 °C | 340 °F | |
Heatbath/Park 400 Quench Oil Similar to AAA but contains extra reservoir of accelerator additive for use in situations where excessive consumption occurs.Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Flash Point | 171 °C | 340 °F | |
Heatbath/Park AAA Quench Oil AAA Quench Oil is the most widely specified accelerated fast oil quenchant. It is ideal for carbon steel and low and medium alloy steel. AAA Quench Oil achieves faster cooling rates through intensi.. |
|||
Flash Point | 171 °C | 340 °F | ASTM D92 |
ChevronTexaco HD Soluble Oil FeaturesChevron Soluble Oils are used broadly in machine shops as multifunctional cutting fluids. They are primarily designed to cool and lubricate the contact point of the tool and the work piece.C.. |
|||
Flash Point | 171 °C | 340 °F | |
ChevronTexaco Crater® A Texaco Crater lubricants delivers value through:Low environmental impact — Contains a carrier solvent that is a non-ozone depleting diluent.Good water resistance — Strong resistance to water washo.. |
|||
Flash Point | 171 °C | 340 °F | ASTM D-92 |
ConocoPhillips Hydroclear® 10 Ultra-Clean Spindle Oil Description: Conoco Hydroclear Ultra-Clean Spindle fluids comprise blends of special base oils and additives specially formulated for use in applications where a lubricant combining the properties o.. |
|||
Flash Point | 171 °C | 340 °F | ASTM D92, ISO 2592 |
Chesterton 690 FG Lubricant Description: Chesterton® 690 FG Lubricant is a high-quality, cost-effective penetrating lubricant. Used in food processing, beverage and pharmaceutical plants, 690 FG Lubricant can go where few pro.. |