Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | -1.11 - 110 °C | 30.0 - 230 °F | Average value: 64.1 °C Grade Count:36 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Flash Point | -1.11 - 200 °C | 30.0 - 392 °F | Average value: 90.3 °C Grade Count:34 |
Overview of materials for Thermoset Polyurethane, Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values .. |
|||
Flash Point | -1.11 °C | 30.0 °F | ASTM D56 |
Humiseal 1A33 Urethane Conformal Coating Humiseal 1A33 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL.. |
|||
Flash Point | -1.11 °C | 30.0 °F | ASTM D56 |
Humiseal 1B12 Acrylic Conformal Coating Humiseal 1B12 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityPasses thermal shock test (MIL-I-46058C)Flammabili.. |
|||
Flash Point | -1.11 °C | 30.0 °F | ASTM D56 |
Humiseal 1B31 Acrylic Conformal Coating Humiseal 1B31 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityMIL-I-46058C ApprovedPasses thermal shock test (MI.. |
|||
Flash Point | -1.11 °C | 30.0 °F | ASTM D56 |
Humiseal 1B73 Acrylic Conformal Coating Humiseal 1B73 Acrylic Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesSelective chemical resistanceExcellent repairabilityUL ApprovedMIL-I-46058C ApprovedPasses thermal sho.. |