Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 126 °C | 259 °F | ASTM D92 |
ExxonMobil Vacmul O 3 D Vacmul O 3 D is a non-staining honing oil recommended for rough and finish honing of safety razor blades. It is suitable for light duty high speed applications and for use in large volume circulatio.. |
|||
Flash Point | 126 °C | 259 °F | ASTM D92 |
ExxonMobil Vacmul O 3 D Vacmul O 3 D is a non-staining honing oil recommended for rough and finish honing of safety razor blades. It is suitable for light duty high speed applications and for use in large volume circulatio.. |
|||
Flash Point | 126 °C | 259 °F | Pensky Martens closed cup |
Dow VORANATE™ T-80 toluene diisocyanate (TDI) VORANATE™ T-80 TDI products are designed for a variety of high-resilience molding, TDI molding, formulating (systems) and flexible slabstock applications. They are used in the production of flexib.. |