Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | -4.00 °C | 24.8 °F | |
Permabond POP Polyolefin Primer Permabond® Polyolefin Primer has been developed for surface treatment of polyolefins, PTFE and silicones prior to bonding with Permabond® Cyanoacrylate adhesives. Due to their low surface energy, .. |
|||
Flash Point | -4.00 - 100 °C | 24.8 - 212 °F | Average value: 33.0 °C Grade Count:4 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Flash Point | -4.00 °C | 24.8 °F | |
LG Chemical Non-Aromatic Raffinate Structure & Characteristics: Produced as a by-product of aromatics extraction process, and is mainly composed of non-aromatics of C6~C8.Uses: Used to blend solvent or gasoline.CAS: 78-78-4, 109-66-0.. |
|||
Flash Point | -4.00 °C | 24.8 °F | Chemlok® 485; Seta |
Lord Adhesives Chemlok® 485/Curative 44 Adhesive LORD Chemlok® 485/Curative 44 adhesive is a two component adhesive system used for insert mold bonding of PVC and Alcryn® to substrates such as metal, rubber and other thermoplastic elastomers.. |
|||
Flash Point | -4.00 °C | 24.8 °F | closed cup |
Dow Corning 92-023 PRIMER Information provided by Dow Corning |
|||
Flash Point | -4.00 °C | 24.8 °F | closed cup |
Dow Corning HV 10 PRIMER Adhesion to aluminium, stainless steel, galvanised steel, epoxy-glass fibre, PFA, good with addition cured silicone rubbers.Information provided by Dow Corning |
|||
Flash Point | -4.00 °C | 24.8 °F | closed cup |
Dow Corning OS-120 Information provided by Dow Corning |
|||
Flash Point | -4.00 °C | 24.8 °F | |
3M C100J Adhesion Promoter 3M™ Adhesion Promoter C100 is a liquid promoter used to improve the adhesion of 3M™ Acrylic Foam Tapes to automotive substrates.Information provided by 3M |
|||
Flash Point | -4.00 °C | 24.8 °F | |
3M Scotch-Seal™ 1252 Tamper Proof Sealant 3M™ Scotch-Seal™ Tamper Proof Sealant 1252 is a fast drying, anti-tamper sealer which is fire retardant.Features: Can be applied over adjustable or removable parts to indicuate changes in adjustme.. |