Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 102 °C | 215 °F | ASTM D56 |
Humiseal 1C49 Silicone Conformal Coating Humiseal 1C49 Silicone Conformal CoatingHigh temperature resistanceGood dielectrical propertiesGood moisture resistanceRepairableUL ApprovedMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-4605.. |