Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 79.0 °C | 174 °F | CC |
LG Chemical Phenol Structure & Characteristics: C6H5OH. Phenol is a white crystalline solid with a distinct smellUses: Raw material of phenolic resins, dye stuffs, synthetic fibers, herbicides, photo material, aromati.. |
|||
Flash Point | 79.0 °C | 174 °F | closed cup |
Dow Corning Z-1216 PHENYLTRICHLOROSILANE Phenyltrichlorosilane fluidInformation provided by Dow Corning |
|||
Flash Point | 79.0 °C | 174 °F | ASTM D92 |
ChevronTexaco 100 NC Open Gear Lubricant FeaturesChevron Open Gear Lubricants are black, viscous lubricants formulated with an asphaltic base and diluted with a nonchlorinated solvent for easy application by hand or through automatic lubri.. |
|||
Flash Point | 78.9 °C | 174 °F | Method A; ASTM D56 |
ExxonMobil Varsol™ 80 Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and EuropeInformation provided by ExxonMobil |
|||
Flash Point | 79.0 °C | 174 °F | |
BASF 2-Ethylhexanoyl Chloride Formula: C8H15ClOCAS: 760-67-8Description: 2-Ethylhexanoyl chloride is a colorless to yellowish liquid with a pungent odor. It is miscible with all common organic solvents. It hydrolyses in the pres.. |