Thermal Properties Metric English Comments
Flash Point >= 55.0 °C
>= 131 °F
nad
Unipetrol Grade 2 Diesel Oil
Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap..
Flash Point >= 55.0 °C
>= 131 °F
nad
Unipetrol Grade B Diesel Oil
Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap..
Flash Point >= 55.0 °C
>= 131 °F
nad
Unipetrol Grade D Diesel Oil
Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap..
Flash Point 55.0 °C
131 °F
closed cup
Dow Corning SYL-OFF® 7069 RELEASE MODIFIER
Syl-Off® 7069 Release Modifier is a 100% active solids, pre-catalysed, release modifier. Pre-catalysed with Rhodium catalyst. General purpose release modifier recommeded for use with Syl-Off® 7044..
Flash Point 55.0 °C
131 °F
Closed Cup
Dow Corning XIAMETER® PMCPPMX-0244 Cyclotetrasiloxane
Is chemically equivalent to DOW CORNING® 244 FLUID. This product is a volatile methylsiloxane fluid, clear, odorless, VOC-exempt, low toxicity, low surface tension and evaporates completely at room..
Flash Point 55.0 °C
131 °F
BASF Ethylene Chlorohydrine
Formula: C2H5ClOCAS: 107-07-3Description: Ethylene chlorohydrine is a colorless liquid, with an alcohol-like odor. It is miscible with water in all proportion.Synonyms: Ethylene chlorhydrin, 2-Chlo..
Flash Point 55.0 °C
131 °F
BorsodChem ONGRONOX EHP 50 D peroxide-type initiator
Chemical name: Bis-(2-ethylhexyl)-peroxi-dicarbonate. Mol. wt: 346.5g/mol. Active oxygen content: 4.62 %. Deflegmation material: isododecane. Major decomposition products: carbon-dioxide, 2-ethyl-he..
Flash Point 55.0 °C
131 °F
BorsodChem ONGRONOX EHP 75 D peroxide-type initiator
Chemical name: Bis-(2-ethylhexyl)-peroxi-dicarbonate.Mol. wt: 346.5g/mol.Active oxygen content: 4.62 %.Deflegmation material: isododecane. Major decomposition products: carbon-dioxide, 2-ethyl-hexan..
Flash Point >= 55.0 °C
>= 131 °F
BASF ptBCF 4-tert.-Butylcyclohexyl choroformate
Formula: C11H19ClOCAS: 42125-46-2Description: ptBCF is a colorless to yellow liquid with a pungent odor.Synonyms: 4-t-Butylcyclohexyl chlormiat, Carbonochloride acid, 4(1,1-dimethylethyl)cyclohexyle..
Flash Point >= 55.0 °C
>= 131 °F
nad
Unipetrol Grade F Diesel Oil
Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap..