Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 61.1 °C | 142 °F | Method A; ASTM D93 |
ExxonMobil Isopar™ J Isoparaffin Fluid Product Description: A clear isoparaffin fluid, typically containing less than 1 ppm benzene and less than 1 ppm sulfur. Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East and Eu.. |
|||
Flash Point | >= 61.1 °C | >= 142 °F | Closed cup |
Dow Corning 2-2647 Performance Modifier Surface active silicone designed for reducing surface tension in silicone emulsions and improving drainage in pulp brownstock washing.Information provided by Dow Corning |