Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 31.0 °C | 87.8 °F | |
Permabond Nitroethane Solvent for Cyanoacrylate The PERMABOND SOLVENT is extremely effective for dissolving cyanoacrylate bonds or removing cured excess adhesive. It is not recommended for use on acrylic plastics. The solvent base is Nitroethane... |
|||
Flash Point | 31.0 °C | 87.8 °F | closed cup |
Dow Corning P5200 ADHESION PROMOTER, CLEAR Dow Corning P5200 Adhesion Promoter is typically applied in a very thin layer to non-porous and porous construction finishes to increase the bonding capacity of Dow Corning silicone construction sea.. |
|||
Flash Point | 31.0 °C | 87.8 °F | closed cup |
Dow Corning P5200 ADHESION PROMOTER, RED Dow Corning P5200 Adhesion Promoter is typically applied in a very thin layer to non-porous and porous construction finishes to increase the bonding capacity of Dow Corning silicone construction sea.. |