Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 304 °C | 579 °F | ASTM D92 |
ChevronTexaco Sil-X® NLGI 1 Grease FeaturesChevron Sil-X Grease is a silica thickened grease. It is manufactured using high viscosity, high viscosity index base oils and contain effective rust and oxidation inhibitors.It is transpare.. |
|||
Flash Point | 304 °C | 579 °F | ASTM D92 |
ChevronTexaco Sil-X® SF Grease FeaturesChevron Sil-X Grease is a silica thickened grease. It is manufactured using high viscosity, high viscosity index base oils and contain effective rust and oxidation inhibitors.It is transpare.. |