Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil 65 Exxon Aviation Oil EE Series Aviation Oil EE is the brand name of a premium quality line of ashless-dispersant piston engine oils. Formulated with select, highly refined base oils together with ashless-dispersant and anti-oxida.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil Mobil Delvac 50 Synthetic Transmission Fluid Mobil Delvac Synthetic Transmission Fluid 50 is a fully synthetic, manual transmission lubricant engineered to meet the most demanding extended drain and OEM warranty requirements. It is recommended.. |
|||
Flash Point | 240 °C | 464 °F | |
ConocoPhillips Syncon® 32 Synthetic AW Hydraulic Fluid 32 Syncon AW Hydraulic Fluid is a premium quality, synthetic antiwear hydraulic fluid developed for use in industrial and mobile equipment operating at extreme temperatures. It is particularly recommen.. |
|||
Flash Point | 240 °C | 464 °F | |
ChevronTexaco 13 SG Diesel Engine Oil Texaco Diesel Engine Oils deliver value through:Ability to maximize oil and filter lifeImproved wear controlExtended drainsExtends oil drains in new low oil consumption GE locomotives, reducing oil .. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ChevronTexaco 46 Heat Transfer Oil FeaturesChevron Heat Transfer Oils are mineral-type transfer oils for use in secondary or indirect heating systems. They are formulated with ISOSYN® base stocks. Chevron Heat Transfer Oils are nont.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ChevronTexaco 7R Unconventional Base Oil FeaturesChevron Unconventional Base Oils (UCBOs) are all hydroprocessed, highly refined paraffinic base oils of exceptional performance and purity.Relative to conventional hydroprocessed and solvent.. |
|||
Flash Point | 240 °C | 464 °F | |
ChevronTexaco Cetus® DE 100 Texaco Cetus DE oils deliver value through:Long life — Texaco Cetus DE oils have a low sludge-forming tendency and a high solvency for deposits that help to keep compressor parts clean. Their abili.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ChevronTexaco FM ISO 46 Synthetic Compressor Oil FeaturesChevron Synthetic Compressor Oil FM is a PAO based, synthetic, food grade, compressor oil.Although Chevron Synthetic Compressor Oil FM offers a reduced risk of fires and explosions, it is no.. |
|||
Flash Point | 240 °C | 464 °F | |
ChevronTexaco Meropa® 150 Texaco Meropa oils deliver value through:Gear set efficiencies — High thermal stability EP system maintains clean gear and bearing surfaces, minimizing deposits which interfere with effective lubri.. |
|||
Flash Point | 240 °C | 464 °F | |
ChevronTexaco Syn-Star® 320 Chain Oil Texaco Syn-Star Chain Oil 320 is a chain oil designed for use in extreme high and low temperature operations. It is formulated with synthetic base oils and an additive package which provides rust an.. |
|||
Flash Point | 240 °C | 464 °F | |
ChevronTexaco Taro® 16 XD SAE 30 Texaco Taro 16 XD delivers value through:Wear protection — Superior antiwear characteristics result in reduced wear on all moving engine components. Controls ring and liner wear through its ability.. |
|||
Flash Point | 240 °C | 464 °F | |
ChevronTexaco Taro® 50 XL SAE 40 Texaco Taro 50 XL delivers value through:Wear protection — Performance results in the latest design medium speed trunk piston diesel engines have shown that the high level of alkalinity of this lub.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ChevronTexaco TEGRA® ISO 460 Synthetic Gear Lubricant FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality industrial EP gear lubricants.The most advanced formulation has been selected to provide superior load carrying and antiwear prop.. |
|||
Flash Point | 240 °C | 464 °F | |
ChevronTexaco Texmar 16 SG SAE 30 Texaco Texmar 16 SG delivers value through:Wear protection — Texaco Texmar 16 SG oil has superior anti-wear characteristics to reduce wear on all moving engine components. Controls ring and liner w.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil 65 Exxon Aviation Oil EE Series Aviation Oil EE is the brand name of a premium quality line of ashless-dispersant piston engine oils. Formulated with select, highly refined base oils together with ashless-dispersant and anti-oxida.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil Mobil Delvac 50 Synthetic Transmission Fluid Mobil Delvac Synthetic Transmission Fluid 50 is a fully synthetic, manual transmission lubricant engineered to meet the most demanding extended drain and OEM warranty requirements. It is recommended.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil Mobil Synthetic Oven Lube 1090 Mobil Synthetic Oven Lube 1090 is a supreme performance synthetic high temperature lubricant designed specifically for lubrication of hot conveyor chains in drying ovens and similar severe applicati.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil Teresstic 68 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D-92 |
ConocoPhillips ANDEROL® 6068 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Flash Point | 240 °C | 464 °F | ASTM D-92 |
ConocoPhillips ANDEROL® 6680 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Flash Point | 240 °C | 464 °F | PMCC; ASTM D92 |
ExxonMobil Synesstic™ 12 Synthetic Fluid Product Description: Synesstic™ Alkylated Naphthalene (AN) represent a unique class of API Group V category fluids. Synesstic™ AN products offer improved hydrolytic, thermal and oxidative stabilit.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil 50 Mobiltrans HD Mobiltrans HD 10W, 30, 50, and 60 are extra high performance transmission and drive-train lubricants engineered to meet the rigorous specifications required by Caterpillar TO-4. This product line .. |
|||
Flash Point | 240 °C | 464 °F | ASTM D-92 |
ConocoPhillips ANDEROL® 6100 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Flash Point | 240 °C | 464 °F | ASTM D-92 |
ConocoPhillips ANDEROL® FGH 22 Synthetic Food Grade Hydraulic Fluid, ISO 22 Description: ANDEROL FGH Series Hydraulic Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA wh.. |
|||
Flash Point | >= 240 °C | >= 464 °F | DIN 51755 |
BASF AH-Salt Recommended use: For the production of homopolymerisates and copolymerisatesInformation provided by BASF |
|||
Flash Point | 240 °C | 464 °F | ASTM D-92 |
ConocoPhillips ANDEROL® FGH 46 Synthetic Food Grade Hydraulic Fluid, ISO 46 Description: ANDEROL FGH Series Hydraulic Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA wh.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil SAE 30 Mobilgard M40 Series Mobilgard M40 Series (M340 and M440) by ExxonMobil are premium, extra high performance 40 TBN engine oils designed for use in the most severe residual-fuelled medium-speed diesel applications found .. |
|||
Flash Point | 240 °C | 464 °F | |
BASF Palatinol® N Diisononyl Phthalate Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D-92 |
ConocoPhillips ANDEROL® FGH 32 Synthetic Food Grade Hydraulic Fluid, ISO 32 Description: ANDEROL FGH Series Hydraulic Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA wh.. |
|||
Flash Point | 240 °C | 464 °F | ASTM D92 |
ExxonMobil 624 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are good performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are for.. |