Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 220 °C | 428 °F | |
LG Chemical LGflex EBNW Plasticizer Features: Excellent Adhesion, Transparency, and Non-endocrine disrupterApplication: PVC Food Package WrapInformation provided by LG Chemical |
|||
Flash Point | 220 °C | 428 °F | ASTM D92 |
ExxonMobil 24 Mobil DTE 20 Series Mobil DTE 20 Series oils are supreme performance anti-wear hydraulic oils designed to satisfy a wide range of hydraulic equipment requirements. They provide long oil/filter life and optimum equipmen.. |
|||
Flash Point | 220 °C | 428 °F | ASTM D92 |
ExxonMobil Teresstic 46 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Flash Point | >= 220 °C | >= 428 °F | ASTM D92 |
ExxonMobil 320 Mobil SHC PM Series Mobil SHC PM Series products are supreme performance synthetic lubricants specifically designed for the most demanding industrial paper machine circulating systems. They are engineered to provide ex.. |
|||
Flash Point | 220 °C | 428 °F | |
ChevronTexaco 32 AW Hydraulic Oil Texaco AW Hydraulic Oils deliver value through:High oxidation stability — Longer service life than with conventional lubricants in high pressure service.Rust and corrosion protection — Gives excel.. |
|||
Flash Point | 220 °C | 428 °F | ASTM D92 |
ChevronTexaco ECO® ISO 68 Hydraulic Oil AW FeaturesChevron ECO Hydraulic Oils AW are environmentally responsible hydraulic oils.They are manufactured from high viscosity index re-refined paraffinic base oils.They provide antiwear protection,.. |
|||
Flash Point | 220 °C | 428 °F | ASTM D92 |
ChevronTexaco Elite-Cut® NM Metal Working Fluid FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met.. |
|||
Flash Point | 220 °C | 428 °F | ASTM D92 |
ChevronTexaco FM ISO 32 Lubricating Oil Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr.. |
|||
Flash Point | 220 °C | 428 °F | |
ChevronTexaco Geotex® LA SAE 15W-40 Texaco Geotex LA oils deliver value through:Low maintenance cost and long engine lifeLow wear — Provide excellent protection againstpiston, ring, and liner scuffing, scoring, and wear.Reduced valve.. |
|||
Flash Point | 220 °C | 428 °F | ASTM D92 |
ChevronTexaco HDAX® SAE 15W-40 Low Ash Gas Engine Oil FeaturesChevron HDAX Low Ash Gas Engine Oils are high quality, bright stock-free, low ash, dispersant/detergent type engine oils.They are formulated with ISOSYN™ base stocks and an additive package.. |
|||
Flash Point | 220 °C | 428 °F | See Note 3. |
ChevronTexaco Marfak® 0 Texaco Marfak grease delivers value through:Good film strengthGood rust and corrosion protection, even in wet conditions.Texaco Marfak greases are fibrous sodium soap greases. It resists oil separat.. |
|||
Flash Point | 220 °C | 428 °F | See Note 3. |
ChevronTexaco Marfak® Heavy Duty 2 Texaco Marfak grease delivers value through:Good film strengthGood rust and corrosion protection, even in wet conditions.Texaco Marfak greases are fibrous sodium soap greases. It resists oil separat.. |
|||
Flash Point | 220 °C | 428 °F | ASTM D92 |
ChevronTexaco Mechanism LPS® ISO 32 Hydraulic Oil Chevron Mechanism LPS Hydraulic Oils are highly refined, paraffinic oils containing oxidation and rust inhibitors, and special antiwear additives to extend the life of hydraulic pumps and motor part.. |
|||
Flash Point | 220 °C | 428 °F | ASTM D92 |
ChevronTexaco Rykon® ISO 32 Oil AW FeaturesChevron Rykon Oils AW are designed to give maximum hydraulic pump protection.Chevron Rykon Oils AW are formulated with ISOSYN® base stocks.They provide excellent antiwear protection, oxidat.. |
|||
Flash Point | 220 °C | 428 °F | COC; ASTM D92 |
ExxonMobil SpectraSyn™ 4 Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn™ Low Viscosity Polyalphaolefin (PAO) basestocks feature low temperature properties, low volatility, and improved thermal stability. SpectraSyn™ Low Viscosity (PAO) .. |
|||
Flash Point | 220 °C | 428 °F | ASTM D92 |
ExxonMobil 24 Mobil DTE 20 Series Mobil DTE 20 Series oils are supreme performance anti-wear hydraulic oils designed to satisfy a wide range of hydraulic equipment requirements. They provide long oil/filter life and optimum equipmen.. |
|||
Flash Point | 220 °C | 428 °F | ASTM D92 |
ExxonMobil Teresstic 46 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Flash Point | 220 °C | 428 °F | ASTM D-92 |
ConocoPhillips ANDEROL® 6460 Synthetic Food Grade Gear Fluid Description: ANDEROL 6000 Series Food Grade Gear Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the .. |
|||
Flash Point | 220 °C | 428 °F | ASTM D-92 |
ConocoPhillips ANDEROL® AA-40 White Mineral Food Grade Oil, ISO Grade 150, SAE Grade 40 Description: ANDEROL PQ AA Series Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Oils are .. |
|||
Flash Point | 220 °C | 428 °F | ASTM D-92 |
ConocoPhillips ANDEROL® HTC Chain & Way Fluid, Synthetic Food Grade ISO 460 Description: ANDEROL HTC Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA where incidental fo.. |
|||
Flash Point | 220 °C | 428 °F | ASTM D-92 |
ConocoPhillips ANDEROL® PQ AA 80 White Mineral Food Grade Gear Oil, ISO Grade 68/100, SAE Gear Oil Grade 80 Description: ANDEROL PQ AA Series Gear Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Gear.. |
|||
Flash Point | 220 °C | 428 °F | COC |
ConocoPhillips Hydroclear Diamond Class® 32 AW Turbine Oil Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser.. |
|||
Flash Point | 220 °C | 428 °F | COC |
ConocoPhillips Hydroclear Diamond Class® 32 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |
|||
Flash Point | 220 °C | 428 °F | |
ChevronTexaco Cygnus® 32 Hydraulic Oil Texaco Cygnus Hydraulic Oils deliver value through:High quality control — Enables customer to use lubricants almost as pure as the food being processedHigh performance — Provides lubrication bette.. |
|||
Flash Point | 220 °C | 428 °F | |
ChevronTexaco Cleartex® D Texaco Cleartex metalworking fluids deliver value through:Multipurpose performance — Texaco Cleartex cutting oils are tri-purpose, serving as the cutting oil, hydraulic fluid and machine lubricant .. |
|||
Flash Point | 220 °C | 428 °F | ASTM D92 |
ChevronTexaco ISO 22 AIO FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring .. |
|||
Flash Point | 220 °C | 428 °F | ASTM D92 |
ChevronTexaco ISO 32 Hydraulic Oil AW FeaturesChevron Hydraulic Oils AW are designed to give excellent hydraulic pump protection. They are formulated with refined paraffinic base oils. They provide excellent antiwear protection, oxidati.. |
|||
Flash Point | 220 °C | 428 °F | |
ChevronTexaco Rando® HD 32 Texaco Rando HD oils deliver value through:Longer equipment life — Special antiwear additive package reduces wear by protecting surfaces when load causes breakdown of the lubricant film.Reduced dow.. |
|||
Flash Point | 220 °C | 428 °F | |
ChevronTexaco Rando® HDZ 32 Texaco Rando HDZ oils deliver value through:High oxidation stability — Longer service life than attainable with conventional lubricants used in high pressure service.Protection against rust and cor.. |
|||
Flash Point | 220 °C | 428 °F | ASTM D92 |
ChevronTexaco Regal® 32 VSI R&O Texaco Regal R&O oils deliver value through:Rust prevention — Prevents rust on surfaces above and below the oil level during long-term storage.Texaco Regal R&O 32 VSI is a fully formulated ISO 32 t.. |