Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 206 °C | 403 °F | |
LG Chemical DOP Plasticizer Applications: Leather, Sheet, Cable, Gloves, Hoses, Footwear, WallpaperInformation provided by LG Chemical |
|||
Flash Point | 206 °C | 403 °F | |
The Chemical Company ChemFlexx™ DOA C22H42O4 Chemflexx DOA is a Dioctyl adipate (DOA) plasticizer. DOA is an ester of 2-ethylhexanol and adipic acid. It is a low-toxicity, biodegradable, light colored, oily liquid generally used as a plasticiz.. |