Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q65B Polyurethane Rubber Sulphur cured, Polyurethane Rubber, 55-65 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG621, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resist.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q70B Polyurethane Rubber Peroxide cured, Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resis.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q70W Polyurethane Rubber Peroxide cured, off-white Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abra.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q70X Polyurethane Rubber Peroxide cured, self-lubricating, Polyurethane Rubber, 65-75 °IRHD. Compounded with graphite or molyb-d. To meet ASTM line call-out M5BG714, B14, EO14, EO34. Polyester-based urethane. ASTM & ISO d.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q70Y Polyurethane Rubber Peroxide cured, yellow Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG714, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasio.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q75B Polyurethane Rubber Sulphur cured, Polyurethane Rubber, 65-75 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG728, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resist.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Precision Polymer Engineering Q90B Polyurethane Rubber Peroxide cured, Polyurethane Rubber, 85-95 °IRHD. Polyester-based urethane. To meet ASTM line call-out M5BG910, B14, EO14, EO34. ASTM & ISO designation = AU.Applications: Excellent abrasion resis.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Indium Corp. Indalloy® 84001 Flux #1 Paste Flux containing Ammonium Chloride Indalloy Flux #1 is a non-acid, non toxic, Pb-free, amber colored paste flux for use on copper, brass, galvanized iron, lead, zinc, tin, silver, nickel, mild steel, terne plate and malleable iron. .. |
|||
Flash Point | >= 204 °C | >= 400 °F | |
Uniseal BETABRACE™ 85076 Epoxy BETABRACE™ 85076 is an expandable composite used for reinforcing sheet metal. It is composed of a high temperature curing tacky polymer, woven glass fabric, and release paper. BETABRACE™ 85076 p.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Westlake Epolene® E-10 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Epolene® E-Type Polymers are easily emulsifiable, available in PE and PP based materials, and approved by the FDA for food contact. They have a wide ring & ball softening point range, oil and water.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Westlake Epolene® E-14E Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Product Description: The Epolene E-14E is a low molecular weight, low density, oxidized polyethylene. The low molecular weight and low softening point contribute to the production of stable, low col.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Westlake Epolene® E-14EP Oxidized Low Molecular Weight Polyethylene Polymer Description: The Epolene E-14EP is a low molecular weight, low density, oxidized polyethylene powder. The low molecular weight and low softening point contribute to the production of stable, low col.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Westlake Epolene® EE-2 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Product Description: EE-2 is a medium density, low molecular-weight oxidized polyethylene with exceptional hardness. It is an excellent asphalt modifier which mixes readily with all asphalts. It h.. |
|||
Flash Point | >= 204 °C | >= 399 °F | Open Cup |
Dow Corning XIAMETER® PMCPPMX-200 20Cs Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 20CS. 100% active, 20 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |
|||
Flash Point | 204 °C | 399 °F | ASTM D92 |
ChevronTexaco ECO® ISO 32 Hydraulic Oil AW FeaturesChevron ECO Hydraulic Oils AW are environmentally responsible hydraulic oils.They are manufactured from high viscosity index re-refined paraffinic base oils.They provide antiwear protection,.. |
|||
Flash Point | 204 °C | 399 °F | ASTM D92 |
ChevronTexaco Open Gear Grease FeaturesChevron Open Gear Greases are formulated with high viscosity mineral oils in a nonsoap-based thickener. These greases appear brownish-black and are extremely tacky.Chevron Open Gear Greases .. |
|||
Flash Point | 204 °C | 399 °F | ASTM D92 |
ChevronTexaco RPM® SAE 75W-90 Synthetic Gear Lubricant FeaturesChevron RPM Synthetic Gear Lubricant is a heavy duty, extreme pressure, multigrade automotive gear lubricant.It is manufactured from synthesized hydrocarbon base fluids which have excellent .. |
|||
Flash Point | >= 204 °C | >= 400 °F | ASTM D93 Closed Cup |
Dow PAPI™ 901 Polymeric MDI PAPI™ 901 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has a high functionality and a high viscosity resulting in highly rigid foams. This product is desi.. |
|||
Flash Point | >= 204 °C | >= 400 °F | ASTM D93 Closed Cup |
Dow PAPI™ 94 Polymeric MDI PAPI™ 901 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This products low viscosity, low functionality, increased diphenylmethane diisocyanate content and increased perc.. |
|||
Flash Point | >= 204 °C | >= 399 °F | Closed Cup; ASTM D93 |
Dow PAPI™ 95 Polymeric MDI PAPI™ 95 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality (value of 2.4) and viscosity have been optimized by maintaining a high diphenylmethan.. |
|||
Flash Point | >= 204 °C | >= 399 °F | |
Dow SPECTRIM™ MM 310-A Isocyanate SPECTRIM™ MM 310-A specialty isocyanate is a component of SPECTRIM™ MM 310 reaction moldable polymer.Information provided by Dow |
|||
Flash Point | 204 °C | 399 °F | ASTM D-92 |
ConocoPhillips ANDEROL® 783-0 Series Synthetic Food Grade Greases, NLGI Grade 0 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |
|||
Flash Point | 204 °C | 400 °F | |
ConocoPhillips Hydroclear® 150 Industrial Oil Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende.. |
|||
Flash Point | 204 °C | 400 °F | |
ConocoPhillips Hydroclear® 22 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Flash Point | 204 °C | 400 °F | |
ConocoPhillips Hydroclear® MV32 AW Hydraulic Fluid Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a.. |
|||
Flash Point | >= 204 °C | >= 399 °F | Closed Cup; ASTM D93 |
Dow PAPI™ 20 Polymeric MDI PAPI™ 20 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product`s functionality value of 3.2 and high viscosity result in highly rigid foams. This product is design.. |
|||
Flash Point | >= 204 °C | >= 399 °F | Closed Cup; ASTM D93 |
Dow PAPI™ 580 N Polymeric MDI PAPI™ 580 N polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has high functionality (value of 3.0) and relatively high viscosity. Recommended for use in polyi.. |
|||
Flash Point | >= 204 °C | >= 399 °F | PMCC |
Dow VORANOL™ VORACTIV™ 6340 Catalytically Active Polyether Polyol VORANOL™ VORACTIV™ 6340 polyether polyol is a catalytically active, high functionality capped polyol. Its high molecular weight, functionality, high primary hydroxyl content, and inherent catalyt.. |
|||
Flash Point | 204 °C | 400 °F | |
ConocoPhillips MV32 Super Hydraulic Oil Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, .. |
|||
Flash Point | >= 204 °C | >= 399 °F | ASTM D92 |
ExxonMobil Mobil Almo 527 Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio.. |