Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | >= 200 °C | >= 392 °F | |
Precision Polymer Engineering E60D Ethylene Propylene Rubber Sulphur cured, Ethylene Propylene Terpolymer, 56-65 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated in accordance with BS2494 Type ‘W’. Water Research Council (WRC) teste.. |
|||
Flash Point | >= 200 °C | >= 392 °F | |
Precision Polymer Engineering E60Q Ethylene Propylene Rubber Peroxide cured, Ethylene Propylene Terpolymer, 60 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States Federal Food .. |
|||
Flash Point | >= 200 °C | >= 392 °F | |
Precision Polymer Engineering E70A Ethylene Propylene Rubber Blue, Ethylene Propylene Terpolymer (EPT), 65-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Formulated using only those ingredients determined by the United States Food and Drug .. |
|||
Flash Point | >= 200 °C | >= 392 °F | |
Precision Polymer Engineering E70E Ethylene Propylene Rubber Ethylene Propylene Terpolymer, 66-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet Aerospace Specification DTD5597A Grade 70.Applications: For sealing applications where goo.. |
|||
Flash Point | >= 200 °C | >= 392 °F | |
Precision Polymer Engineering E70V Ethylene Propylene Rubber Peroxide cured, blue-violet Ethylene Propylene Terpolymer, 65-75 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing applications involving high voltage .. |
|||
Flash Point | >= 200 °C | >= 392 °F | |
Precision Polymer Engineering E80K Ethylene Propylene Rubber General purpose, peroxide cured, Ethylene Propylene Terpolymer, 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. To meet ASTM D2000/SAE J200 line call-out MCA810, A25, B35, F17... |
|||
Flash Point | >= 200 °C | >= 392 °F | |
Precision Polymer Engineering E80V Ethylene Propylene Rubber Peroxide cured, blue-violet coloured Ethylene Propylene Terpolymer, 75-85 °IRHD. Terpolymer of ethylene, propylene and diene monomers. Specially formulated for sealing applications involving high.. |
|||
Flash Point | 200 °C | 392 °F | ASTM D92 |
ExxonMobil Fenso 51 FENSO is the brand name for a series of premium quality oils designed specially for use as heat-treating fluids. The FENSO line consists of two grades: one medium-viscosity, dual-purpose oil for bot.. |
|||
Flash Point | 200 °C | 392 °F | |
ExxonMobil Mobil Clean 10W-30 7500 Mobil Clean 7500 is formulated from a combination of synthetic and conventional quality base stocks combined with modern performance additives, including an advanced cleaning additive system to prov.. |
|||
Flash Point | 200 °C | 392 °F | |
ExxonMobil Mobil Clean 10W-40 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
Flash Point | 200 °C | 392 °F | |
ExxonMobil Mobil Clean 5W-30 7500 Mobil Clean 7500 is formulated from a combination of synthetic and conventional quality base stocks combined with modern performance additives, including an advanced cleaning additive system to prov.. |
|||
Flash Point | 200 °C | 392 °F | |
ExxonMobil Mobil Clean 5W-30 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
Flash Point | 200 °C | 392 °F | |
ExxonMobil Mobil Clean 5W-30 5000 Mobil Clean 5000 is formulated from high quality base stocks combined with modern performance additives, including an advanced detergent system to provide excellent engine cleanliness at oil drain i.. |
|||
Flash Point | 200 °C | 392 °F | ASTM D-92 |
ConocoPhillips ANDEROL® PQ AA 1000 White Mineral Food Grade Gear Oil, ISO Grade 1000, SAE Gear Oil Grade 1000 Description: ANDEROL PQ AA Series Gear Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Gear.. |
|||
Flash Point | 200 °C | 392 °F | |
ExxonMobil Mobil Clean 10W-30 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
Flash Point | 200 °C | 392 °F | |
BASF Lupranate® 5050 Isocyanate Description: Lupranate® 5050 Isocyanate is a prepolymer based on a modified, pure MDI. The intermediate free-NCO and slightly enhanced functionality of Lupranate 5050 isocyanate has benefited the f.. |
|||
Flash Point | 200 °C | 392 °F | |
BASF Lupranate® 5140 Isocyanate Description: Lupranate® 5140 Isocyanate is a prepolymer based on a modified, pure MDI. The intermediate free-NCO and enhanced functionality of Lupranate 5140 isocyanate has benefited the formulatio.. |
|||
Flash Point | >= 200 °C | >= 392 °F | ASTM D1929 |
BASF Neopolen® 1710 100 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |
|||
Flash Point | >= 200 °C | >= 392 °F | ASTM D1929 |
BASF Neopolen® 1712 100 mm Expanded Polyethylene Uses: Foam plates for the production of packaging, sporting goods and technical components.Information provided by BASF |
|||
Flash Point | >= 200 °C | >= 392 °F | ASTM D1929 |
BASF Neopolen® P 9225 K 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Flash Point | >= 200 °C | >= 392 °F | ASTM D1929 |
BASF Neopolen® P 9225 K 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9225 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9225 K.Note: In order to.. |
|||
Flash Point | >= 200 °C | >= 392 °F | ASTM D1929 |
BASF Neopolen® P 9230 D 0.05 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |
|||
Flash Point | >= 200 °C | >= 392 °F | ASTM D1929 |
BASF Neopolen® P 9235 0.04 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea.. |
|||
Flash Point | 200 °C | 392 °F | |
BASF Lupranate® 259 Isocyanate Description: Lupranate® 259 Isocyanate is a modified pure MDI. No 259 Isocyanate is applicable for use in all CASE applications.Information provided by BASF |
|||
Flash Point | 200 °C | 392 °F | |
BASF Lupranate® 5070 Isocyanate Description: Lupranate® 5070 Isocyanate is a low functional prepolymer based on pure MDI. Lupranate 5070 isocyanate is favored in solid elastomers and microcellular foams where the formulator desir.. |
|||
Flash Point | 200 °C | 392 °F | |
ExxonMobil Mobil Clean 20W-50 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
Flash Point | 200 °C | 392 °F | |
BASF Lupranate® LP30 Isocyanate Description: Lupranate® LP30 isocyanate is a solvent-free, modified pure diphenylmethane diisocyanate which is liquid at 30°C. It is designed to replace pure MDI in applications where it is desira.. |
|||
Flash Point | >= 200 °C | >= 392 °F | |
BASF Lupranate® M10 Isocyanate Description: Lupranate® M10 Isocyanate is a solvent-free polymeric MDI with a functionality of approximately 2.3. Lupranate M10 Isocyanate is a polymeric MDI which contains a relatively high level .. |
|||
Flash Point | >= 200 °C | >= 392 °F | ASTM D1929 |
BASF Neopolen® P 9230 D 0.07 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to.. |