Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 199 °C | 390 °F | |
Lubriplate 32 Turbine Oil Petroleum-Based Air Compressor Fluid This high-performance, zinc-free fluid meets the requirements of most centrifugal air compressors. Provides excellent oxidation resistance. Turbine Oil 32 is available in Drums.Information provided .. |
|||
Flash Point | 199 °C | 390 °F | |
Lubriplate APG-250 Petroleum-Based Gear, Bearing, & Recirculating Oil These heavy-duty, EP (extreme pressure) type oils were developed to meet gear oil needs of most automotive, truck, heavy equipment, and industrial gear boxes requiring an extreme pressure. Meets mil.. |
|||
Flash Point | 199 °C | 390 °F | |
Lubriplate NO. 3 NO.3 Petroleum-Based Machine Tool Oil Compounded to impart a unique load carrying film, exceptional lubricity, and anti-friction properties not found in conventional oils of the same viscosity. Machine Tool Oils are available in Bottles.. |
|||
Flash Point | 199 °C | 390 °F | COC; ASTM D92 |
ExxonMobil Exterex™ A34 Synthetic Fluid Product Description: Esterex™ Adipate Esters are API category Group V fluids. These esters have excellent low-temperature properties, high viscosity indices, good lubricating properties and low vol.. |
|||
Flash Point | 199 °C | 390 °F | |
BASF Lupranate® 227 Isocyanate Description: Lupranate® 227 Isocyanate is a liquid, modified blend product based on isomers of diphenylmethane diisocyanate (MDI). This product has good storage stability at room temperature and of.. |
|||
Flash Point | 199 °C | 390 °F | |
BASF Lupranate® 265 Isocyanate Description: Lupranate® 265 Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate 265 Isocyanate is used in the i.. |
|||
Flash Point | 199 °C | 390 °F | |
BASF Lupranate® MI Isocyanate Description: Lupranate® MI Isocyanate is pure diphenylmethane diisocyanate containing a higher amount of 2,4´ isomer than Lupranate M Isocyanate or Lupranate MS Isocyanate. Lupranate MI Isocyanate.. |
|||
Flash Point | 199 °C | 390 °F | |
BASF Lupranate® MM103 Isocyanate Modified MDI Description: Lupranate® MM103 is a liquid carbodiimide modified 4,4’-diphenylmethane diisocyanate. Lupranate MM103 serves as the isocyanate component in the production of microcellular urethane el.. |
|||
Flash Point | 199 °C | 390 °F | |
BASF Lupranate® MS Isocyanate Description: Lupranate® MS, a solid at room temperature, is essentially pure MDI and has a functionality of 2.0. Lupranate MS isocyanate is used in the isocyanate component for the preparation of e.. |
|||
Flash Point | 199 °C | 390 °F | |
BASF Lupranate® MT Isocyanate Description: Lupranate® MT Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate® MT Isocyanate is used in the .. |
|||
Flash Point | 199 °C | 390 °F | |
BASF Lupranate® MTD Isocyanate Description: Lupranate® MTD Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate® MTD Isocyanate is used in the.. |
|||
Flash Point | 199 °C | 390 °F | |
BASF Lupranate® 234 Isocyanate Description: Lupranate® 234 Isocyanate is a low functionality (approximately 2.3) low viscosity polymeric MDI with high 2,4’-MDI isomer content. Lupranate® 234 Isocyanate exhibits excellent low t.. |
|||
Flash Point | 199 °C | 390 °F | |
BASF Lupranate® 241 Isocyanate Description: Lupranate® 241 Isocyanate is a low functionality (approximately 2.3) low viscosity polymeric MDI with high2,4’-MDI isomer content. Lupranate® 241 Isocyanate exhibits excellent low t.. |
|||
Flash Point | 199 °C | 390 °F | |
BASF Lupranate® 78 Isocyanate Description: Lupranate® 78 Isocyanate is a polymeric MDI with a functionality of approximately 2.3. This product exhibits excellent low temperature stability. Lupranate 78 Isocyanate will remain a .. |
|||
Flash Point | 199 °C | 390 °F | |
BASF Lupranate® 81 Isocyanate Description: Lupranate® 81 Isocyanate is a carbodiimide modified pure MDI with a higher 2,4’-isomer content and a functionality of approximately 2.1. Lupranate 81 Isocyanate exhibits good low temp.. |
|||
Flash Point | 199 °C | 390 °F | |
BASF Lupranate® M Isocyanate Description: Lupranate® M Isocyanate, a solid at room temperature, is essentially pure 4,4´-diphenylmethane diisocyanate, having a functionality of 2.0. Lupranate M Isocyanate is used in the isoc.. |
|||
Flash Point | 199 °C | 390 °F | |
BASF Lupranate® MS/264 Isocyanate Description: Lupranate® MS/264, a solid at room temperature, is essentially pure MDI and has a functionality of 2.0. Lupranate MS/264 isocyanate is used in the isocyanate component for the preparat.. |
|||
Flash Point | 199 °C | 390 °F | |
BASF Lupranate® 5143 Isocyanate Description: Lupranate® 5143 isocyanate is a liquid, carbodiimide-modified 4,4’-diphenylmethane diisocyanate. With manufacturing advances, Lupranate 5143 isocyanate achieves better low temperature.. |