Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 13.0 °C | 55.4 °F | |
Lord Adhesives 202 Semi-Flexible, Fast Cure, Medium Viscosity Acrylic Adhesive Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f.. |
|||
Flash Point | 13.0 °C | 55.4 °F | |
Lord Adhesives 510 Fast Cure Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Flash Point | 13.0 °C | 55.4 °F | |
Lord Adhesives 551 Very Low Viscosity, Adhesive Thinner, Medium Cure Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Flash Point | 13.0 °C | 55.4 °F | closed cup |
Dow Corning C2-0563 REPELLENT An air-drying, air-curing silicone fabric finish for natural and synthetic fabrics.Information provided by Dow Corning |
|||
Flash Point | 13.0 °C | 55.4 °F | closed cup |
Dow Corning Z-6032 SILANE DOW CORNING Z6032 contains a vinylbenzyl and amine organic and a trimethoxysilyl inorganic group. The product is supplied in methanol. Possessing both organic and inorganic reactivity, DOW CORNING Z.. |
|||
Flash Point | 13.0 °C | 55.4 °F | closed cup |
Dow Corning Z-6224 SILANE Dow Corning® Z-6224 Silane contains vinylbenzyl and amine organic groups and methoxysilyl inorganic reactivity. The product is supplied in methanol. It is the neutralized (low chloride) version of .. |
|||
Flash Point | 13.0 °C | 55.4 °F | closed cup |
Dow Corning 1205 RTV PRIME COAT Clear, film forming primer for use with all silicone RTVsInformation provided by Dow Corning |
|||
Flash Point | 13.0 °C | 55.4 °F | closed cup |
Dow Corning 1200 OS PRIMER CLEAR Adhesion to metals, ceramics, rubbers, PVC's, polyesters, PET, acrylics, PUInformation provided by Dow Corning |
|||
Flash Point | 13.0 °C | 55.4 °F | Closed cup |
Dow Corning 531 Fluid 50% active, amino methoxy functional polydimethylsiloxane in solvent.Information provided by Dow Corning |
|||
Flash Point | 13.0 °C | 55.4 °F | |
BASF Pivaloyl Chloride Formula: C5H9ClOCAS: 3282-30-2Description Pivaloyl chloride is a colorless to light yellow liquid with a pungent odor. It hydrolyses in the presence of water.Synonyms: Trimethylacetyl chloride, Neo.. |