Thermal Properties | Metric | English | Comments |
---|---|---|---|
Flash Point | 119 °C | 246 °F | closed cup |
Dow Corning Z-6228 SILANE Dow Corning® Z-6228 Silane is a dialkyldimethoxysilane. Silanes and siloxanes have been used for some time in this application to increase yield and improve the stereoregularity of the polyolefin r.. |
|||
Flash Point | 119 °C | 246 °F | Method A; ASTM D93 |
ExxonMobil Exxsol™ D120 Dearomatized Fluid Availability: Africa & Middle East and Europe Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil |