Thermal Properties Metric English Comments
Flash Point -37.0 °C
-34.6 °F
BASF Isopropylamine
Formula: C3H9NCAS: 75-31-0Description: Isopropanolamine is a colorless to yellowish liquid with an amine-like odor. It is miscible in water.Synonyms: 1-Amino-2-propanol, Monoisopropanolamin, 1-Amin..