Boiling Point 240 - 244 °C
464 - 471 °F
BASF 1,5-Pentanediol (PDO)
Formula: C5H12O2CAS: 111-29-5Description: 1,5-Pentanediol (PDO) is a colorless, oily liquid with characteristic odor. It is miscible in water and organic solvents.Synonyms: 1,5-Dihydroxypentane, 1,5..