Thermal Properties | Metric | English | Comments |
---|---|---|---|
Boiling Point | 4800 °C | 8670 °F | |
CMW® ELKON 100M Pure Molybdenum Molybdenum (ELKON® 100M) is a refractory metal that resembles tungsten in many respects. Its hardness, melting, and boiling temperatures are only slightly lower than those of tungsten are. The elec.. |